After the polypropylene fibrillated fiber is put into the concrete, the transverse connection between the fiber monofilaments can be destroyed by the rubbing and friction of the concrete itself, forming the fiber monofilament or network structure fully opening.
 
 
polypropylene fibrillated fiber
 
Construction method of polypropylene mesh fiber: after the polypropylene mesh fiber is put into the concrete, in the process of concrete mixing, the transverse connection between the fiber monofilaments can be destroyed by the rubbing and friction of the concrete itself, forming the fiber monofilament or mesh structure fully opening, so as to realize the effect of a large number of polypropylene fiber monofilaments to prevent cracking.
 
 
 
Length selection: 19mm for ordinary concrete and 10mm for shotcrete. In general, the mixing amount is 0.9kg/m3, that of deck waterproof layer is 0.9-1.8kg/m3, and that of Shotcrete for tunnel is 0.9-1.8kg/m3.
 
 
 
Mixing process: first put gravel, then fiber, and then put sand to stir for 2 minutes, so that the fiber is fully opened, and then put in cement and water, and mix evenly according to the conventional process.

CONTACT US

QQ: 278686715

Phone: +86-18678313600

Tel: +86-543-5779757

Email: 278686715

Add: No.23,Road Longfeng,Town Lizhuang ,County Huimin,Shandong,China ,251700

Scan the qr codeClose
the qr code